MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crosspolimeri EPIGUM ME/15 P 2ZS Modified Rubber Technopolymers
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Epigum: is the trade-mark of our modified rubber technopolymers presenting many of the positive features of pure rubbers and plastic materials : lead free

Epigum ME/15 P 2ZS: they present good deformation and compression resistance and have a good resistance properties to flex-fatigue and to abrasion. Also good resistance to the fuels. They conserve their flexibility and elasticity in a big range of temperatures.

Certify: AS/NZ 3808 Type 5V-90

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666ASTM D2240
Tensile Strength 12.5 MPa1810 psiIEC 60811
 9.375 - 15.625 MPa
@Temperature 115 °C,
Time 1.81e+6 sec
1360 - 2266.2 psi
@Temperature 239 °F,
Time 504 hour
Heat Ageing; AS 1660
Elongation at Break 250 %250 %IEC 60811
 187.5 - 312.5 %
@Temperature 115 °C,
Time 1.81e+6 sec
187.5 - 312.5 %
@Temperature 239 °F,
Time 504 hour
Heat Ageing; AS 1660
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 90.0 °C
@Time 21600 sec
194 °F
@Time 6.00 hour
<50%, Penetration
 
Processing PropertiesMetricEnglishComments
Zone 1 140 °C284 °F
Zone 2 145 °C293 °F
Zone 3 150 °C302 °F
Zone 4 155 °C311 °F
Die Temperature 170 °C338 °F
Head Temperature 165 °C329 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS050 / 294134

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.