MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess PUROLAN® E 171 A Titanium Dioxide Pigment
Categories: Ceramic; Oxide; Titanium Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: PUROLAN® E 171 A is suitable for the pigmentation of cosmetics, foodstuffs and others. The respective national legislations have to be observed. PUROLAN® E 171 A is used in cosmetics e.g. in covering creams (lipsticks; makeup) and body powder. PUROLAN® E 171 A is readily dispersible and has good lightening power.

INCI: Titanium Dioxide

CAS No.: 13463-67-7

EINECS No.: 236-675-5

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.80 g/ccISO 787 Part 10
Loss On Ignition <= 1.0 %
Particle Size 0.26 µmd50
pH 7.0 - 8.5
Specific Surface Area 9.0 m²/g
Evaporation Loss <= 5.0 %
@Temperature 105 °C
Drying
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
 
Component Elements PropertiesOriginal ValueComments
Arsenic, As <= 0.00010 %Extraction with 0.5 n HCI
Cadmium, Cd <= 0.00010 %Extraction with 0.5 n HCI
Lead, Pb <= 0.0010 %Extraction with 0.5 n HCI
Mercury, Hg <= 0.00010 %Extraction with 0.5 n HCI
TiO2 >= 99 %
 
Descriptive Properties
AppearanceWhite to almost white powder
Content<0.5%Acid-Soluble Substances
 <0.5%Water-Soluble Substances
 <12mg/kgAntimony (Sb), Extraction with 0.5 n HCI
Specifications0-1Tone, PLV b
 98-98.9Brightness, PLV L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Dioxide, Rutile
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Overview of materials for Polystyrene, Glass Filled
Overview of materials for Polystyrene, Extrusion Grade
Covestro Arcol® E-434 Polyether Polyol

PLANY8153 / 208546

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.