MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Polystone® M MPG Glass filled UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:
  • Low coefficient of friction
  • Long service life
  • Superior abrasion & wear resistance
Product applications:
  • Chute and hopper liners
  • Dragline bucket liners
  • Wearstrips

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
Water Absorption <= 0.010 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63 - 96ASTM D2240
Tensile Strength, Yield 2700 psiASTM D638
Elongation at Break >= 265 %ASTM D638
Tensile Modulus 100000 psiASTM D638
Compressive Strength 3000 psiASTM D695
Izod Impact, Notched (ISO) 110 kJ/m²ASTM D4020
Coefficient of Friction, Dynamic 0.10 - 0.22Dry vs. Steel
Coefficient of Friction, Static 0.15 - 0.20Dry vs. Steel
Sand Slurry 82
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+12 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µin/in-°FASTM D696
Melting Point 266 - 275 °F
Maximum Service Temperature, Air 180 °F
Flammability, UL94 HB
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
FDA No
NSF No
USDA No
 
Descriptive Properties
ColorMedium Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
Techmer ES HiFill® HDPE GF30 30% Glass Filled
Omni Plastics OmniTech™ HDPE GRC30 High Density Polyethylene, 30% Glass Reinforced
Polymer Industries Polyslick UHMW Profile

PROCH005 / 66209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.