MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Torlon® 4000T PAI, Coarse powder for compounding
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: Coarse powder for compounding, available in low, medium and high viscosities

Torlon® 4000T is a neat resin polyamide-imide (PAI) coarse powder designed for compounding with other polymers and specialty additives. It is the base resin utilized in all Torlon injection molded compounds. Its powder form enables designers to enhance custom compounds and specialty applications with the well-known properties of Torlon polyamide-imide, from its unstoppable performance under extreme conditions to excellent resistance against wear, creep and chemicals.

A fine-particle powder version, Torlon® 4000TF, is also available, which is particularly well suited for compression molded parts. A water soluble analog of Torlon® 4000T is available as Torlon® AI-50.

Torlon® 4000T has been shown to be useful in blends with polyphenylsulfone (PPSU), polyethersulfone (PES), polysulfone (PSU), polyetheretherketone (PEEK), high-temperature sulfone resins, self-reinforced polyphenylene, polybenzimidizole (PBI), polyimide (PI), polyetherimide (PEI), and polyphenylene sulfide (PPS). Besides blending with other polymers to enhance properties, Torlon® 4000T powder may be compounded with a wide variety of performance fillers, reinforcements, specialty additives and colorants to meet the desired need. The resultant compound may then be injection molded or extruded into film, shapes or fiber.

In addition to molded components, Torlon® PAI powders are suitable for use in other high performance forms. For example, these powders are soluble in dipolar aprotic solvents such as N-methyl pyrrolidone (NMP), dimethylacetamide (DMAC), dimethylsulfoxide (DMSO) and dimethylformamide (DMF). Solutions of these systems can be sprayed into coatings, cast into films, spun into fibers and cast or spun into specialty membranes. High strength, high temperature capable adhesives can be also formulated from Torlon® PAI powders. Torlon® PAI powders may be incorporated into epoxy and other thermoset systems to provide additional strength, ductility and heat resistance.

Torlon® 4000T powders are available in 3 viscosity grades, which are defined by the inherent viscosity (IV) ranges shown in the accompanying data.

- Low viscosity: 4000T-LV
- Medium viscosity: 4000T-MV
- High viscosity: 4000T-HV

Markets/Uses: Coatings / High Performance Coatings / Abrasion Resistant Coatings; Coatings / High Performance Coatings / Corrosion Resistant Coatings; Coatings / High Performance Coatings / High-Temperature Coatings; Coatings / High Performance Coatings / Primers for Non-Stick Coatings

Applications: Blending; Cast Film; Coating Applications

Features: Chemical Resistant; Flame Retardant; High Heat Resistance

Injection notes: Drying Time/Temp: 4 hrs. @ 300°F
Drying Time/Temp: 16 hrs.@ 250°F

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Processing PropertiesOriginal ValueComments
Drying Temperature 177 °C
@Time 10800 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPowder
ProcessingCoating; Compounding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4542 / 280342

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.