MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineering properties in combination with excellent dimensional stability, low warp and resistance to sink-mark-formation. It is ideally suited for applications such as rotors, wheels, rims, timing belt covers, automotive cooling fans, shrouds as well as interior and exterior door handles.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.51 g/ccISO 1183
Viscosity Measurement 142ISO 307
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 250 MPa
@Load 3.06 kg
ISO 2039-2
Tensile Strength, Yield 140 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 10500 MPaISO 527-2
Flexural Strength 210 MPaISO 178
Flexural Modulus 8700 MPaISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-2
Decomposition Temperature >= 300 °C
Ignition Temperature >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 270 °CFeed Zone
Zone 2 280 °CCompression
Zone 3 290 °CMetering-zone
Zone 4 290 °CNozzle
Melt Temperature 280 - 300 °CInjection Molding/Extrusion
 290 °COptimal
Mold Temperature 80.0 °COptimal
 80.0 - 90.0 °CInjection molding
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 00130
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
Domo Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)

PBASG0405 / 132038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.