MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow LDPE 4005 Low Density Polyethylene, Extrusion Coating Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: DOW Polyethylene 4005 extrusion coating resin is used in highly demanding packaging applications such as pharmaceuticals, dried fruits, and meats. The low density and high molecular weight of LDPE 4005 allow it to heat seal easily and maintain a high heat seal strength. It complies with U.S. FDA regulation 21 CFR 177.1520 c 2.1 for food contact applications. The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.916 g/cc
Melt Flow 5.5 g/10 min
@Load 2.16 kg
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 88.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LDPE 4012 Low Density Polyethylene, Extrusion Coating Grade
Dow LDPE 5004I Low Density Polyethylene, Extrusion Coating Grade
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade
Dow LDPE 4005M Low Density Polyethylene

PDW488 / 34557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.