MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carmel Olefins Capilene® E 50 E Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: CAPILENE® E 50 E is a low melt flow rate polypropylene homopolymer intended for extrusion, thermoforming and blow molding featuring very good process ability and melt stability. Products manufactured with CAPILENE® E 50 E are characterized by a very good stiffness and impact balance.

APPLICATIONS

CAPILENE ® E 50 E is mainly used in the in-line extrusion-thermoforming process for the production of cups and containers. Other extrusion applications are foils, sheets, strapping, slit film yarn for textile, ropes, chenille and nets.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 31.0 MPa4500 psiASTM D638
Elongation at Yield 14 %14 %ASTM D638
Flexural Modulus 1.40 GPa203 ksiASTM D790
Izod Impact, Notched 0.500 J/cm
@Temperature >=23.0 °C
0.937 ft-lb/in
@Temperature >=73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FASTM D648
Vicat Softening Point 152 °C
@Load 1.02 kg
306 °F
@Load 2.25 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carmel Olefins Capilene® W 77 AV Polypropylene Homopolymer
Braskem Prisma® 6410 Extrusion Blow Molding Polypropylene
Braskem H 603 Extrusion Polypropylene Homopolymer
Braskem H 203 Fiber Extrusion Polypropylene Homopolymer
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion

PCARM019 / 79757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.