MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Duracon® CH-20 CD3501 Acetal Copolymer, CF
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: Electric conductive. 20% carbon fiber reinforced. Low wear.

Information provided by Polyplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Filler Content 20 %20 %Carbon fiber
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
0.0030 in/in
@Thickness 0.0787 in
Cavity pressure 60 MPa; 60x60x2; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
0.0090 in/in
@Thickness 0.0787 in
Cavity pressure 60 Mpa; 60x60x2; ISO 294-4
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ISO 2039-2
Tensile Strength 144 MPa20900 psiISO 527-1,2
Elongation at Break 1.5 %1.5 %ISO 527-1,2
Tensile Modulus 14.0 GPa2030 ksiISO 527-1,2
Flexural Strength 205 MPa29700 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
Coefficient of Friction, Dynamic  0.24
@Pressure 0.490 MPa
0.24
@Pressure 71.1 psi
Thrust, vs C-Steel. 30 cm/s; JIS K7218
 0.39
@Pressure 0.0600 MPa
0.39
@Pressure 8.70 psi
Thrust, vs M90-44. 15 cm/s; JIS K7218
K (wear) Factor  5.00 x 10-8 mm³/N-M
@Pressure 0.490 MPa
2.48 x 10-10 in³-min/ft-lb-hr
@Pressure 71.1 psi
Thrust, vs C-Steel, steel side. 30 cm/s; JIS K7218
 100 x 10-8 mm³/N-M
@Pressure 0.0600 MPa
49.6 x 10-10 in³-min/ft-lb-hr
@Pressure 8.70 psi
Thrust, vs M90-44, material side. 15 cm/s; JIS K7218
 300 x 10-8 mm³/N-M
@Pressure 0.490 MPa
149 x 10-10 in³-min/ft-lb-hr
@Pressure 71.1 psi
Thrust, vs C-Steel, material side. 30 cm/s; JIS K7218
 10000 x 10-8 mm³/N-M
@Pressure 0.0600 MPa
4960 x 10-10 in³-min/ft-lb-hr
@Pressure 8.70 psi
Thrust, vs M90-44, M90-44 side. 15 cm/s; JIS K7218
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 ohm-cm100 ohm-cmStandard test
Surface Resistance 50 ohm50 ohmStandard test
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
@Temperature 73.4 - 131 °F
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °FISO 75-1,2
Flammability, UL94 HBHB
 
Descriptive Properties
Yellow Card File No.E213445

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPL9821 / 305494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.