Product Description: QGel 313 is a clear, soft, tough, moderately cross-linked silicone polymer. This product is a two-component material with a 20:1 mix ratio by weight or by volume. It can also be mixed at a 10:1 ratio by weight or by volume which will yield a harder gel. Key Features: - 20:1 mix ratio
- Greater than 7 day room temperature work life
- Dispensing equipment not necessary
- Heat cure required
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |