MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® POM 770/1 SI2 POM, 2% Silicone
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Silicone Filled

Material Notes: Base Polymer: Polyoxymethylene Copolymer

Filler/Additive System: 2% silicone

Special Features: Heat ageing stabilization, improved sliding/wear

Market Segment: Automotive, Machinery

Application Area: Gear wheels, roller bearings

Typical Applications: Functional components, bearings and sliding elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.020 - 0.021 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 - 0.021 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 112 MPaH358/30; ISO 2039-1
Tensile Strength, Yield 48.0 MPaISO 527
Elongation at Break 51 %ISO 527
Tensile Modulus 2500 MPaISO 527
Flexural Strength 57.0 MPaISO 178
Flexural Modulus 2310 MPaISO 178
Charpy Impact Unnotched 115 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.10 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 169 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CISO 75-1/-2
Vicat Softening Point 145 °CB50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 220 °CInjection molding
Mold Temperature 60.0 - 120 °CInjection molding
Drying Temperature 100 - 110 °C
@Time 7200 - 10800 sec
in a dry air (desiccant) dryer
 100 - 110 °C
@Time 10800 - 18000 sec
in air circulating dryer
 
Descriptive Properties
Base PolymerPolyoxymethylene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALCOM® POM 770/1 MO2 POM, 2% MoS2 Reinforced
Asahi Kasei TENAC™ 2010 Homopolymer Acetal (POM), High viscosity
Mocom (ALBIS) ALCOM® POM 770/1 PTFE18 SI2 POM, 20% PTFE/Silicone
Mocom (ALBIS) ALCOM® POM 770/1 GF20 PTFE15 POM, 20/15% Glass/PTFE Reinforced
Mocom (ALBIS) ALCOLOR® Function POM LE A BK1226-07 Color additive

PALBIS8189 / 242248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.