MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® M855 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: CHR® M-Series (5 Mil PET with Adhesive) are manufactured from polyester film with either rubber or silicone pressure-sensitive adhesive.

Features/Benefits: Polyester backings offer low cost effective holding for materials and resist damage from sharp edges. M855 rubber adhesive is specially formulated to use as a flash mask protection tape in metal or composite bonding. The non-silicone adhesive eliminates silicone contamination and is specially formulated to remove cleanly from most surfaces after up to 4.0 hours at 177 °C. Polyester backing resists damage from sharp edges, and protects tool surfaces from abuse and adhesive flash in vacuum bag sealing. Also, polyester backings offer low cost, effective positioning tape for composite lay-ups prior to bag sealing. This tape will function at temperatures up to 130 °C.

Applications: M855 Polyester film offers an economical method to hold, insulate and/or protect materials.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 100 %
Tear Strength 100 pliInitial Tear Strength
Peel Strength 0.0700 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 10000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air 0.000 °F
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray
Master Bond MasterSil 800 One Component, Room Temperature Curing Silicone
Henkel Loctite® 5248 Silicone Adhesive
Dynasol Calprene® 401 Thermoplastic Rubber SBS Dry
CHT Group QSil 440 Condensation Cure Silicone Adhesive

PSTGQZ325 / 68839

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.