MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling OPTAMID® Cast Polyamide 6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Application: deflection rope sheaves for elevators

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: PA 6 G
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO R 1183
Moisture Absorption at Equilibrium 2.2 %2.2 %DIN 53473
Water Absorption at Saturation 7.0 %
@Temperature 20.0 °C
7.0 %
@Temperature 68.0 °F
ISO R 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 120 MPa17400 psiHc 30; ISO 2039; partially
Tensile Strength, Yield 60.0 MPa8700 psiISO-DIS 527
Creep Strength 11.0 MPa1600 psi1% elongation, 1000 h; DIN 53444
 15.0 MPa2180 psi2% elongation, 1000 h; DIN 53444
Tensile Modulus 2.70 GPa392 ksiDIN 53457
Flexural Strength 55.0 MPa7980 psiDIN 54352
Flexural Modulus 2.40 GPa348 ksiDIN 53457
Izod Impact, Notched (ISO) >= 15.0 kJ/m²>= 7.14 ft-lb/in²DIN 53453
Izod Impact Resistance NBNBswinging hammer 0,1 DIN 51222; DIN 53453
Coefficient of Friction 0.0800.080With lubrication
Coefficient of Friction, Dynamic 0.420.42no lube; Steel 2162, Rvst=2E-6m, p=0.05 Mpa, v=0.6 m/s, t=40°C
Tear Strength Test >= 0.25>= 0.25ISO-DIS 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmDIN 53482
Surface Resistance 1.00e+10 ohm1.00e+10 ohmDIN 53482
Dielectric Constant 3.73.7DIN 53483
Dielectric Strength 20.0 kV/mm508 kV/inDIN 53481
Dielectric Loss Index 0.0300.030DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 80.0 µm/m-°C
@Temperature 20.0 - 100 °C
38.9 - 44.4 µin/in-°F
@Temperature 68.0 - 212 °F
DIN 53752
Specific Heat Capacity 1.67 J/g-°C0.399 BTU/lb-°F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FISO R 1218
Maximum Service Temperature, Air 120 °C248 °FContinuous
 180 °C356 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FV-notch; ISO R 75
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FV-notch; ISO R 75
Minimum Service Temperature, Air -40.0 °C-40.0 °FContinuous
 
Descriptive Properties
Creepage/leakage ResistanceKA3bDIN 53480
Friction Wear0.09 micron/km

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Luriblend® PA6/6 TS20 HS Nylon 66
Techmer ES Luriblend® PA6/6 TL20 HS L Nylon 66
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled
Röchling OPTAMID® Cast Polyamide 6, Dry
PolyPLASTY PolyTAN 15/90 Polyurethane

PSCHW033 / 90230

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.