MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Trigonox 123-C75 Acrylics tert-Amyl peroxyneodecanoate
Categories: Other Engineering Material

Material Notes: Trigonox 123-C75 is used as an initiator for acrylonitrile and (meth)acrylates.

CAS number: 68299-16-1

EINECS/ELINCS No: 64741-65-7

Applications: Trigonox 123-C75 is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc
@Temperature -10.0 °C
0.0322 lb/in³
@Temperature 14.0 °F
Half-life  0.100
@Temperature 81.0 °C
0.100
@Temperature 178 °F
[hr]
 1.00
@Temperature 61.0 °C
1.00
@Temperature 142 °F
[hr]
 10.0
@Temperature 43.0 °C
10.0
@Temperature 109 °F
[hr]
Viscosity 13.7 cP
@Temperature -10.0 °C
13.7 cP
@Temperature 14.0 °F
Storage Temperature -25.0 - -15.0 °C-13.0 - 5.00 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 20.0 °C68.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay74.0 -76.0 %
Color= 50 Pt-Co
Content= 0.10 %Hydroperoxides as TAHP
 = 250 mg/kgInorganic + organic hydrolysable chloride
 4.58-4.71 %Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY999 / 286522

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.