MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, the PVDF membranes has excellent mechanical strength and flexibility. It can not be eroded by acid, alkali, strong oxidant, halogens. Good durability to aliphatic hydrocarbons, aromatic hydrocarbons, alcohol, aldehyde etc. In the work of hydrochloric acid, nitric acid, sulfuric acid, dilute alkali liquor, dense alkali liquor (40%) and 100°C, which keep stable. Others, 904 PVDF finished products has the properties of gamma-Ray resistant, UV (ultraviolet) resistant, and stability in wide temperature range.

Information provided by Shanghai Ofluorine Chemical Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.77 - 1.79 g/ccASTM D792
Water Absorption 0.10 %Drying loss method
Viscosity >= 0.45 cP
@Temperature 30.0 °C
1g/ml MNP, Rotary Viscosity
Viscosity Test 140 - 190 cm³/gIntrinsic Viscosity
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 168 °C10°C/min; ASTM D3418
 
Descriptive Properties
AppearanceWhite powder
SolubilitySolution is clear and transparent, no impurity and insoluble matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group EP MAP-7.5 EPI Engineered Polymers Aliphatic Prepolymer
CHT Group EP AOSR EPI Engineered Polymers Acrylic Oligomer
Chosun Refractories MF-2 Blast Furnace Tap-Hole Refractory
Bakelite® PF 85 Phenolic Formaldehyde Resin, UL Listed
Bakelite® PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets

PSHANGO04 / 130335

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.