MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Cristal™ AN004 Natural Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ copolyester AN004 Natural contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but Eastman Cristal™ copolyester AN004 Natural maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Its processability coupled with its outstanding chemical resistance makes it well suited for thick-wall applications.

Applications

  • Bottles-color cosmetics pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Personal care & cosmetics packaging
Key Attributes
  • Easy to extrude, cut, print, and seal
  • Effective barrier properties
  • Excellent chemical resistance
  • Excellent clarity
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Toughness

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.00200 - 0.00600 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D785
Tensile Strength at Break 46.0 MPaISO 527
 51.0 MPaASTM D638
Tensile Strength, Yield 47.0 MPaISO 527
 47.0 MPaASTM D638
Elongation at Break 200 %ISO 527
 320 %ASTM D638
Elongation at Yield 4.00 %ISO 527
 5.00 %ASTM D638
Flexural Yield Strength 65.0 MPaISO 178
 69.0 MPaASTM D790
Flexural Modulus 2000 MPaASTM D790
Izod Impact, Notched 40.0 J/m
@Temperature -40.0 °C
ASTM D256
 80.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 4.80 kJ/m²
@Temperature -40.0 °C
ISO 180
 7.80 kJ/m²
@Temperature 23.0 °C
ISO 180
Puncture Energy 42.0 J
@Temperature 23.0 °C
@ Max. Load; ASTM D3763
 48.0 J
@Temperature -40.0 °C
@ Max. Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 0.300 %ASTM D1003
Transmission, Visible 89.0 %Regular; ASTM D1003
 91.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 280 °C
Mold Temperature 15.0 - 30.0 °C
Drying Temperature 70.0 °C
Dry Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4020 / 323643

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.