MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese ZENITE 5244L LCP, 40% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled

Material Notes: Zenite 5244L is a 40% glass/mineral reinforced LCP resin with improved toughness.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.71 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 131 MPa5mm/min; ISO 527-2/1A
Elongation at Break 1.66 %5mm/min; ISO 527-2/1A
Tensile Modulus 14000 MPa50mm/min; ISO 527-2/1A
Flexural Strength 198 MPaISO 178
Flexural Modulus 13100 MPaISO 178
Izod Impact, Notched (ISO) 28.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 27.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 16.6 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.18
@Frequency 2.05e+9 Hz
Dissipation Factor 0.040
@Frequency 2.05e+9 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 6.00 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 48.0 µm/m-°CISO 11359-2
Melting Point 318 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °CISO 75-1, -2
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °Ccavity
Feed Temperature 40.0 - 60.0 °C
Zone 1 320 - 330 °C
Zone 2 335 - 345 °C
Zone 3 335 - 345 °C
Zone 4 335 - 345 °C
Die Temperature 335 - 345 °C
Melt Temperature 325 - 345 °C
Drying Temperature >= 150 °C
Dry Time 3.00 hour
Moisture Content <= 0.010 %
Injection Pressure 50.0 - 150 MPa
Hold Pressure 50.0 - 150 MPa
Back Pressure <= 3.00 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese ZENITE 6244L LCP, 40% Mineral / Glass Reinforced
Celanese VECTRA A435 LCP, 35% Specialty
Celanese VECTRA A430 LCP, 25% Specialty
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese VECTRA A230 LCP, 30% Specialty

PHCQ536 / 178991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.