MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synthos IM868 CPE Resin
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CPE is one of the most important impact modifiers for the universal plastics market. Compared with other impact modifiers like AIM (Acrylic Impact Modifier), MBS and ABS.

Characteristics: High molecular weight, superior mechanical performance, high absorption capacity to filler, high performance/cost efficiency.

Application: Specially for PVC pipe application, such as PVC pressure pipe, drain pipe and electrical conduit, etc.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.530 g/cc
Volatiles 0.20 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 58
Tensile Strength 12.0 MPa
Elongation at Break 830 %
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 0.800 J/g
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 35 %
 
Descriptive Properties
AppearanceWhite powder
Content8 piece/100gImpurity particles
Sieve residue00.8mm sieve
Thermal stability time10 minat 165°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW242 / 320273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.