MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bangtai 63E85 Polyester Based TPU for Extrusion Molding
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Processing: Extrusion molding

Properties: Easily processed, smooth and bright with excellent physical properties

Applications: Shoe soles, Shoe insoles, Garden Horses, Reinforced Horse, Solid core wire, Electrical wires and cables, Escalator handrails, Mechanical transmission belts, Surfing ropes, LED light strings, Elastics, Pneumatic tubes, Hair ties etc

Information provided by Baoding Bangtai Polymeric New-materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 - 1.24 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83 - 87ASTM D2240
Tensile Strength 30.0 - 40.0 MPaASTM D412
Elongation at Break 550 - 850 %ASTM D412
100% Modulus 2.00 - 8.00 MPaASTM D412
300% Modulus 8.00 - 14.0 MPaASTM D412
Tear Strength 100 - 160 kg(f)/cmASTM D624
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 200 °C
Drying Temperature 100 - 110 °C
Dry Time 1.00 - 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBANGT012 / 312372

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.