MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products DP-11-75 Urethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: DP-11-75 is a two component medium viscosity urethane patch system. A hybrid product which was designed specifically for making quick responsive repairs/buildups to the MB 4000 Foundry Plank. DP-11-75 is exceptionally tough, highly machinable after cure, and exhibits superior properties similar to MB 4000.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 200 cPPart A
 1600 cPPart B
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 - 30.0 min
Pot Life 1.5 min
@Temperature 24.0 °C
20 gram mass
 
Descriptive Properties
ColorBrownPart A
 RedPart B
Mix Ratio1:1 by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
Overview of materials for Thermoset Polyurethane, Liquid

PBCC014 / 107241

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.