MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 22HSP BK Nylon 66, General Purpose
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Vydyne 22HSP BK is a general-purpose, unfilled, lubricated, heat stabilized PA66 resin. Designed principally for injection-molding fabrication, this product offers a combination of engineering properties characterized by high strength; rigidity; good toughness; high melt point; good surface lubricity; abrasion resistance; and resistance to many chemicals, machine and motor oils, solvents and gasoline. This product is designed to resist thermal degradation when exposed to warm climates.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 48.0 MPa50% RH; ISO 527-2
 81.0 MPaDAM; ISO 527-2
Tensile Strength, Yield 57.0 MPa50% RH; ISO 527-2
 89.0 MPaDAM; ISO 527-2
Elongation at Break 25 %DAM; ISO 527-2
 76 %50% RH; ISO 527-2
Elongation at Yield 4.8 %DAM; ISO 527-2
 20 %50% RH; ISO 527-2
Tensile Modulus 1600 MPa50% RH; ISO 527-2
 3100 MPaDAM; ISO 527-2
Flexural Strength 29.0 MPa50% RH; ISO 178
 102 MPaDAM; ISO 178
Flexural Modulus 1100 MPa50% RH; ISO 178
 3200 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 3.90 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 4.10 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 4.10 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 4.70 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 8.40 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 2.70 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 2.80 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 2.80 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 3.30 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 4.10 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
PLC 6; ASTM D 495
Comparative Tracking Index 400 - 599 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minUL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 195 °CUnannealed; 50% RH; ISO 75-2/B
 208 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CUnannealed; DAM; ISO 75-2/A
 83.0 °CUnannealed; 50% RH; ISO 75-2/A
UL RTI, Electrical 140 °C
@Thickness 0.710 mm
UL 746
 140 °C
@Thickness 1.50 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 95.0 °C
@Thickness 0.710 mm
UL 746
 110 °C
@Thickness 1.50 mm
UL 746
 110 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 115 °C
@Thickness 0.710 mm
UL 746
 125 °C
@Thickness 1.50 mm
UL 746
 125 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.710 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
Flame Spread 0.000 mm/min
@Thickness 2.00 mm
ISO 3795
Oxygen Index 24 %DAM; EN ISO 4589-2
Glow Wire Ignition Temperature 700 °C
@Thickness 0.710 mm
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 825 °C
@Thickness 0.710 mm
IEC 60695-2-12
 825 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °CInjection
Middle Barrel Temperature 270 - 285 °CInjection
Front Barrel Temperature 280 - 290 °CInjection
Nozzle Temperature 280 - 300 °CInjection
Melt Temperature 285 - 300 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature <= 70.0 °CInjection
Dry Time 1.00 - 3.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA0121
 ASTM, D6779 PA0121
 FED, L-P-410A
 MIL, M-20693B
 RoHS Compliant
 SAE, J1639 PA0121 Z6
AppearanceBlack
Automotive Material SpecificationChrysler MS-DB-41 CPN1899
 Delphi M5507
 GM GMW16036P-PA66
 GM QK 002921
 Mercedes-Benz DBL 5410
 VW 50180
FeaturesAbrasion Resistance
 Chemical Resistant
 Fast Molding Cycle
 Gasoline Resistant
 General Purpose
 Good Mold Release
 Good Toughness
 Heat Stabilized
 High Rigidity
 High Strength
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Outdoor Suitabilityf1UL 746C
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 101L BKB009 PA66
Celanese Zytel® 101L BKB080 PA66
Ascend Performance Materials Vydyne® R515J NT0689 Nylon 66, 15% Glass Filled
BASF Ultramid® A3WG7 BK00564 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3W PA66 (Dry)

PASCE9749 / 220852

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.