MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Redwood Plastics Redco™ 430 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Our most commonly used material, ideal for environments where high abrasion resistance is the primary concern. Redco™ 430 (90A) also offers superior impingement resistance.

Standard Color: Yellow

Features: Weather Resistant, Cut & Tear Resistant, Impact Resistant, Elasticity

Typical Applications: Shock and vibration pads, roll covers, springs, cylinder cushions, carriage bumpers, cable sheave liners, deflector plates, impact wear liners, belt scrapers, seals, couplings, washers, cones, impellers, liner plates, pump liners, valve gates, stabilizers, desilter cones, cleaner cones, wear slides, wheels & pulley lagging, protective chute liners, impact pads, slurry-parts, spouts, wear liners, springs, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85 - 9585 - 95
Tensile Strength 36.0 - 37.9 MPa5220 - 5500 psi
Elongation at Break 430 - 587 %430 - 587 %
100% Modulus 7.60 - 8.80 MPa1100 - 1280 psi
300% Modulus 15.2 - 16.3 MPa2200 - 2360 psi
Resilience 42 - 6242 - 62DIN, Bashore
Tear Strength 102 - 105 kN/m582 - 599 pliAngle, Die C
Compression Set 17 - 30 %17 - 30 %Method B
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW022 / 296588

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.