MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Corbion Luminy L175 PLA, Biobased Polymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Luminy L175 is a high heat, high viscosity, PLA homopolymer suitable for film extrusion, thermoforming or fiber spinning.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccLiterature Value
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-A
 8.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133-A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50.0 MPaISO 527-1
Elongation at Break <= 5.0 %ISO 527-1
Tensile Modulus 3500 MPaISO 527-1
Charpy Impact Unnotched <= 5.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 60.0 °CAmorphous; ISO 75-1
 100 - 110 °CCrystalline; ISO 75-1
Glass Transition Temp, Tg 55.0 - 60.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Feed Temperature 20.0 - 40.0 °C
Die Temperature 190 - 210 °C
Dry Time 4.00 - 6.00 hour
@Temperature 100 °C
Moisture Content <= 0.040 %Coulometric Karl-Fischer
 
Descriptive Properties
AppearanceCrystalline white pelletsVisual
Residual Monomer<0.3%Total Corbion PLA Method
Stereochemical Purity>99% (L-isomer)Total Corbion PLA Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer
Total Corbion Luminy LX175 PLA, Biobased Polymer
Total Corbion Luminy L130 PLA, Biobased Polymer
Total Corbion Luminy D070 PLA, Biobased Polymer
Total Corbion Luminy LX175U PLA, Biobased Polymer

PTOTAC003 / 209621

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.