MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
Linear Mold Shrinkage, Transverse 0.0085 - 0.0115 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa
@Temperature 150 °C
 75.0 MPa
@Temperature 120 °C
 100 MPa
@Temperature 90.0 °C
 105 MPa
@Temperature 60.0 °C
 110 MPa
@Temperature 23.0 °C
Elongation at Break 2.0 %
@Temperature 23.0 °C
 2.0 %
@Temperature 60.0 °C
 2.0 %
@Temperature 90.0 °C
 5.0 %
@Temperature 120 °C
 12 %
@Temperature 150 °C
Elongation at Yield 3.5 %
@Temperature 120 °C
 10 %
@Temperature 150 °C
Tensile Modulus 2000 MPa
@Temperature 150 °C
 4400 MPa
@Temperature 120 °C
 5700 MPa
@Temperature 90.0 °C
 6800 MPa
@Temperature 60.0 °C
 7200 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 17.0 kJ/m²
@Temperature -20.0 °C
 20.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
 4.00 kJ/m²
@Temperature -20.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 135 °C
Deflection Temperature at 0.46 MPa (66 psi) 280 °C
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
Vicat Softening Point 265 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 330 °C
Mold Temperature 150 - 170 °C
Drying Temperature 120 - 130 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese CoolPoly® E3607 Thermally Conductive Polyamide (PA6)
Celanese CoolPoly® E3603 Thermally Conductive Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
DuPont Mobility and Materials Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA)

PLATH9620 / 177316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.