Notes: This compound is intended for use in medical and healthcare applications, particularly for extruded medical tubing. This is a specialty grade designed for improved weldability using the Terumo process. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Bondability; Ethylene Oxide Sterilizable; Good Processing Stability; High Clarity; High Purity; Kink Resistant; No Animal Derived Components; Radiation (Gamma) Resistant Uses: Medical/Healthcare Applications; Pharmaceuticals Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |