MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 29.9.R Covered electrodes
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 29.9.R is a covered electrode with rutile basic coating and about 110% metal recovery giving a duplex (ferritic austenitic) all weld metal. It is used for welding of dissimilar materials, high carbon and manganese steels like tool steels as well as surfacing. Sandvik 29.9 R is also used for overlays on hot forming steels and as a universal electrode for repair and maintenance work. Scaling resistant up to 1150 C (2100 F). Spray transfer gives a bead with a finely rippled surface. Little spatter and very good slag removal.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 220
Tensile Strength, Ultimate 720 MPa
Tensile Strength, Yield 600 MPa
@Strain 0.2 %
Elongation at Break 25 %
Reduction of Area 25 %
Charpy Impact 50.0 J
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.010 %
Chromium, Cr 28.5 %
Manganese, Mn 1.5 %
Nickel, Ni 10 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.080 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5149 / 199713

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.