MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro DUREFLEX® A4700 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: Dureflex A4700 is a self-priming, polyether based, low modulus aliphatic thermoplastic polyurethane film/sheet product.

Properties / Applications: Dureflex A4700 was developed as part of a series of optical grade adhesive films. Dureflex A4700 was specifically developed for the lamination of optically transparent glass-clad polycarbonate. Dureflex A4700 is also used in acrylic composites CAB and other compatible thermoplastics. Dureflex A4700 can be supplied from 15 mils to 50 mils (.38 to 1.27 mm) with a specially developed film finish to allow for evacuation of trapped air during press or autoclave bonding. Dureflex A4700 is supplied with a protective polyethylene interleaf to prevent film-to-film roll blocking, and should be incorporated where a “primerless ” lamination is required. As with any product, use of Dureflex A4700 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878ASTM D2240
Tensile Strength, Ultimate 37.9 MPa5500 psiMD/CD Ave; ASTM D882
100% Modulus 3.45 MPa
@Strain 100 %
500 psi
@Strain 100 %
MD/CD Ave; ASTM D882
300% Modulus 10.3 MPa
@Strain 300 %
1490 psi
@Strain 300 %
MD/CD Ave; ASTM D882
Tear Strength 43.8 kN/m250 pliMD/CD Ave; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
Softening Point 76.0 - 100 °C169 - 212 °FASTM E2347-004
 
Descriptive Properties
AppearanceOptically Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnFlex™ HT 40A-3S2131 Thermoplastic Elastomer (TPE)
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester
Austin Novel Materials Texalan® 265A Polyester-based TPU
Covestro Desmodur® XP 2619 Polyurethane
Covestro DESMODURE® N 100A Polyurethane

PCOVEST0759 / 202542

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.