MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Wacker Powersil® 740 DARK GRAY A/B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 740 DARK GRAY A/B is a paste-like, two-component compound with short curing times. Its vulcanizates are noted for high tracking and erosion resistance, their good mechanical properties especially for high tear strength as well as for their excellent dielectric behavior.

Special features:

  • outstanding dielectric properties
  • high tracking and erosion resistance
  • excellent hydrophobic properties
  • very easy to process
  • high tear strength and high elongation
  • excellent mechanical properties
Application:
  • cable accessories
  • insulators
  • outdoor and indoor use

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-1 A
Viscosity  400000 cP
@Shear Rate 10.0 1/s
400000 cP
@Shear Rate 10.0 1/s
Component B; ISO 3219
 425000 cP
@Shear Rate 10.0 1/s
425000 cP
@Shear Rate 10.0 1/s
Mix; ISO 3219
 450000 cP
@Shear Rate 10.0 1/s
450000 cP
@Shear Rate 10.0 1/s
Component A; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ISO 868
Tensile Strength at Break 9.80 MPa1420 psiISO 37
Elongation at Break 670 %670 %ISO 37
Tear Strength 38.0 kN/m217 pliASTM 624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Dielectric Constant 2.9
@Frequency 50 Hz
2.9
@Frequency 50 Hz
IEC 60250
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243
Dissipation Factor 0.00040
@Frequency 50 Hz
0.00040
@Frequency 50 Hz
IEC 60250
Arc Resistance 300 sec300 secIEC 61621
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 31 %31 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
post-cured 4hr at 200°C
Pot Life 4320 min4320 min
 
Descriptive Properties
Colorgray
Track Resistance1A 4.5IEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 4305/65 batch Silicone Rubber
Wacker Elastosil® R plus 4070/30 Silicone Rubber
Wacker Elastosil® R plus 4020/50 Silicone Rubber
Wacker Elastosil® R plus 4001/30 Silicone Rubber
Wacker Elastosil® R plus 4000/60 Silicone Rubber

PWACK9383 / 204912

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.