MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Label-Lyte™ 50LGT702 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A transparent biaxially oriented polypropylene film coated one side resistant coating and one side with a specially formulated acrylic coating. This film is designed for cut and stack labeling. 50LGT702 must be printed in reverse on the static resistant coating, which offers good anchorage to gravure and flexography solvent-based inks, as well as UV curing inks. The film is available in reels (sheets from distributors).

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Superior stiffness
  • High transparency
  • Outstanding static resistant properties
  • Excellent reverse printability of static resistant side
  • Easy cutting into individual labels
  • High gloss finish
  • Excellent anchorage of hot-melts
Features:
  • Static Resistant Coated
Applications:
  • Beverage, Alcoholic
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Health and Beauty Care
  • Industrial
Uses:
  • Cut & Stack (Hot Melt) Labels
Processing Method: Offset Ebeam Printing, Solvent Flexographic Printing, Solvent Rotogravure Printing, UV Flexographic Printing, UV Offset Lithography Printing and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milExxonMobil Method
Coating Weight 29.0 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 175 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 65 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 290 ksiMD; ExxonMobil Method
 508 ksiTD; ExxonMobil Method
Coefficient of Friction 0.23Inside/Outside
Film Tensile Strength at Break, MD 17400 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 35500 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
Shrinkage, TD 2.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 2.5 %ExxonMobil Method
Gloss 83 %45°, Acrylic Surface; ExxonMobil Method
 
Descriptive Properties
Yield14900 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing
Quartz (SiO2)
Hardwire 12x-4-12 Low Density Composite
EFI Composites Featherlite FL4005A Aluminum Trihydrate/Thermoplastic Microspheres
Chengdu Polyster PP Film PP Films/Sheets

PEX99581 / 175817

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.