MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petropol Durepol® A3 V20 CNZ0350 BT331 PBT, 20% Glass Bead Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Bead Filled

Material Notes: Resin ID (ISO 1043): PBT
Color: Gray
Processing: Injection Molding

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccASTM D1238
Linear Mold Shrinkage 0.012 - 0.016 cm/cmASTM D955
Melt Flow 34 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 60.0 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Tensile Modulus 3300 MPaASTM D638
Charpy Impact Unnotched 25.0 kJ/m²ASTM D256
Charpy Impact, Notched 3.50 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 180 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 270 °CMolding
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 120 °C
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL000 / 312908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.