MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible crosslinkable pipes.

BorPEX HE 2515 is designed for the requirements in DIN 16892/BIN 16887 for hot water pressure pipes, e.g. floor heating, radiator connections and for domestic hot and cold water supply. Documentation is available on request.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccISO 1183
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 18.0 MPaAt 50 mm/min; ISO/DIS 6259
Tensile Strength, Yield 3916 psiAt 50 mm/min; ISO/DIS 6259
Elongation at Break 195 %ISO/DIS 6259
Elongation at Yield 11 %ISO/DIS 6259
Modulus of Elasticity 0.960 GPaISO 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature -20.0 °C
ASTM D696
 140 µm/m-°C
@Temperature 20.0 °C
ASTM D696
 500 µm/m-°C
@Temperature 100 °C
ASTM D696
Specific Heat Capacity 2.10 J/g-°C
Vicat Softening Point 126 °CISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Borealis HE1878 High Density Polyethylene Powder for Crosslinked Pipes
Borealis HE1878E High Density Polyethylene Powder for Crosslinked Pipes
Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes

PBOREA016 / 27323

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.