MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C19210, O50 Temper, Sheet
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Light Anneal

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Coated Metal Arc Welding, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Butt Weld

Common Fabrication Processes: Forming and Bending; Heading and Upsetting; Piercing and Punching; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical uses: Cooling Fins for Radiators; Air Conditioning Tubing; Connectors; IC Lead Frames; Terminals; Cooling Fins for Heavy Duty Radiators; Heat Exchanger Tubing; Heat Resistant Applications

Applicable Specifications: Strip – ASTM B888/B88M; Strip, Sheet & Plate – ASTM B465

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 296 MPa
@Thickness 0.457 mm
43000 psi
@Thickness 0.0180 in
Tensile Strength, Yield 152 MPa
@Thickness 0.457 mm
22000 psi
@Thickness 0.0180 in
0.2% Offset
Elongation at Break 38 %
@Thickness 0.457 mm
38 %
@Thickness 0.0180 in
Tensile Modulus 125 GPa18200 ksi
Machinability 20 %20 %
Forgeability 65 %65 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000220 ohm-cm0.00000220 ohm-cm80% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.9 µm/m-°C
@Temperature 20.0 - 300 °C
9.40 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Melting Point <= 1080 °C<= 1980 °F
Liquidus 1080 °C1980 °F
Annealing Point 449 - 549 °C840 - 1020 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 704 - 899 °C1300 - 1650 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99.8 - 99.9 %99.8 - 99.9 %As Balance
Iron, Fe 0.050 - 0.15 %0.050 - 0.15 %
Phosphorus, P 0.025 - 0.040 %0.025 - 0.040 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC19210x1 / 292882

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.