MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lion Diene™ 55AC15 Polymerized rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Diene™55AC15 is a solution polymerized plastics grade medium cis polybutadiene, featuring excellent color and low gel. It is intermediate in solution viscosity and contains a non-volatile and TNPP-free antioxidant system. Diene™ 55AC15 is widely used as an impact modifier for thermoplastic resins such as HIPS and ABS.

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Volatiles <= 0.60 %<= 0.60 %ASTM D5668
Viscosity 147 - 177 cP147 - 177 cP5.43% in Toluene; ASTM D445
Brookfield Viscosity  177000 cP
@Temperature 100 °C
177000 cP
@Temperature 212 °F
RVT #7
 1.90e+6 cP
@Temperature 60.0 °C
1.90e+6 cP
@Temperature 140 °F
RVT #7
Mooney Viscosity 48 - 56
@Temperature 100 °C
48 - 56
@Temperature 212 °F
ML/4; ASTM D 1646
Molecular Weight 47000 g/mol47000 g/molGPC
Ash <= 0.20 %<= 0.20 %ASTM D5667
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -96.0 °C-141 °FASTM E1356
 
Descriptive Properties
Color0-10APHA, ASTM D1209
Content<0.01%Toluene Insolubles
Dissolving Time<4 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLION056 / 317965

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.