MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® TPU 810/4073 AR10 TPU, 10% Aramid Powder Reinforced
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Base Polymer: Polyurethane, Estertype

Filler/Additive System: 10% Aramid Powder

Special Features: Improved sliding/wear

Market Segment: Automotive, Machinery

Typical Application: bearings and sliding elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Maximum Moisture Content 0.050
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87
@Time 15.0 sec
ISO 868
Hardness, Shore D 32
@Time 15.0 sec
ISO 868
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 245 °CInjection molding
Mold Temperature 20.0 - 50.0 °CInjection molding
Drying Temperature 60.0 - 110 °C
@Time 3600 - 10800 sec
in a dry air (desiccant) dryer
 60.0 - 110 °C
@Time 3600 - 10800 sec
in an circulating dryer
 
Descriptive Properties
Base PolymerPolyurethane, Estertype

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALCOM® TPU 810-3070.1 CF15 TPU, 15% Carbon Fiber Reinforced
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
Abatron MasterMold 12-3 Flexible Mold Making Compound
Abatron KromaKote 8901-8 Polyurethane Coating

PALBIS8580 / 242639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.