MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Water Absorption 0.20 %
@Thickness 3.18 mm
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cmASTM D955
Melt Flow 8.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 65.5 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 40 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2520 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 89.6 MPaASTM D790
Flexural Modulus 2520 MPaASTM D790
Izod Impact, Notched 69.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 86.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 188 - 210 °C
Mold Temperature 48.9 - 82.2 °C
Drying Temperature 82.2 °C
Dry Time 2.00 hour
 
Descriptive Properties
AppearanceBlack
FeaturesCopolymer
 General Purpose
 Good Wear Resistance
 Low Friction
FormsPellets
Generic MaterialAcetal (POM) Copolymer
Generic NameAcetal (POM) Copolymer
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Bearings
 Business Equipment
 Consumer Applications
 Gears
 General Purpose
 Industrial Applications
 Pulleys
 Rollers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® AT-15CF/000 BLACK Acetal (POM) Copolymer
Avient LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer
Avient Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
Avient LubriOne™ AT-000/20T Black Acetal (POM) Copolymer
Avient LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer

PH0POL0711 / 145280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.