MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL LDF 723-S Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: MARPOL® LDF 723-S is a homopolymer resin suitable for use in molding, extrusion, compounding and foam applications. This grade contains Slip additive.

Recommended Applications: Foams and injection molding

Additives: Slip – no; Antiblock – 750 ppm.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D1505
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 750 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84ASTM D2240
Hardness, Shore D 45ASTM D2240
Tensile Strength at Break 9.50 MPaASTM D638
Tensile Strength, Yield 10.0 MPaASTM D638
Elongation at Break >= 800 %ASTM D638
Elongation at Yield 40 %ASTM D638
Flexural Modulus, 1% Secant 214 MPaASTM D790
Dart Drop, Total Energy 17.5 J
@Temperature 23.0 °C
ASTM D3763
 26.0 J
@Temperature -40.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 °CPeak; ASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO103 / 283700

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.