J6 Polymers JFOAM™ G-504 Engineered Specialty Foam
Categories:
Polymer
;
Thermoset
;
Polyurethane, TS
;
Thermoset Polyurethane Foam, Unreinforced
Material Notes:
JFoam™ G-504 is a two component water blown polyurethane foam system used in structural panels, as well as in insulation, buoyancy, and potting applications.
Information provided by J6 Polymers LLC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.0641
g/cc
0.00231
lb/in³
Molded, Overall
Viscosity
310
cP
@Temperature 48.9 °C
310
cP
@Temperature 120 °F
T Component
435
cP
@Temperature 43.3 °C
435
cP
@Temperature 110 °F
T Component
620
cP
@Temperature 37.8 °C
620
cP
@Temperature 100 °F
T Component
870
cP
@Temperature 32.2 °C
870
cP
@Temperature 90.0 °F
T Component
1325
cP
@Temperature 26.7 °C
1325
cP
@Temperature 80.0 °F
T Component
1750
cP
@Temperature 21.1 °C
1750
cP
@Temperature 70.0 °F
T Component
1850
cP
@Temperature 48.9 °C
1850
cP
@Temperature 120 °F
R Component
2750
cP
@Temperature 43.3 °C
2750
cP
@Temperature 110 °F
R Component
5250
cP
@Temperature 37.8 °C
5250
cP
@Temperature 100 °F
R Component
7500
cP
@Temperature 32.2 °C
7500
cP
@Temperature 90.0 °F
R Component
15000
cP
@Temperature 26.7 °C
15000
cP
@Temperature 80.0 °F
R Component
26000
cP
@Temperature 21.1 °C
26000
cP
@Temperature 70.0 °F
R Component
Storage Temperature
18.3
-
29.4
°C
65.0
-
85.0
°F
Mechanical Properties
Metric
English
Comments
Compressive Strength
0.379
MPa
55.0
psi
Perpendicular, 10% deflection; ASTM D1621
0.517
MPa
75.0
psi
Parallel, 10% deflection; ASTM D1621
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.0331
W/m-K
0.230
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
82.2
°C
180
°F
Processing Properties
Metric
English
Comments
Shelf Life
6.00
Month
6.00
Month
Descriptive Properties
Closed Cell Content
95%
ASTM D2856
Mixing Ratio
0.36
R Component Water Blown Polyol
0.64
T Component TDI Prepolymer
Water Absorption
0.07 lb/ft2
ASTM D2842
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® TR-20 Polyurethane Foam
ITW Insulation TRYMER® 200L Polyisocyanurate Foam
PJSIX027 / 190954
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.