MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Thermx® CG933 PCT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced

Material Notes: Thermx« CG933 is a 30% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.63 g/ccISO 1183
Moisture Absorption 0.150 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.90 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 119ISO 2039-2
Tensile Strength at Break 114 MPa5mm/min; ISO 527-2/1A
Elongation at Break 1.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 10800 MPa50mm/min; ISO 527-2/1A
Flexural Strength 172 MPaISO 178
Flexural Modulus 10000 MPaISO 178
Charpy Impact Unnotched 30.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 33.0 kV/mmIEC 60243-1
Comparative Tracking Index 440 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 6.00 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-2
Melting Point 285 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 270 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1, -2
Flammability, UL94 V-2
@Thickness 0.800 mm
 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °Ccavity
Melt Temperature 295 - 310 °C
Drying Temperature >= 95.0 °C
Dry Time 4.00 - 6.00 hour
Moisture Content <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Thermx® CG933 NC010 PCT
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Celanese VECTRA C130 LCP, 30% Glass Reinforced
Celanese VECTRA V143XL LCP, 42% Glass Reinforced
Celanese VECTRA S625 LCP, 25% Specialty

PHCQ465 / 178920

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.