MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® MDF603 Nylon 6, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Notes: MDF603 is a 15% glass fiber reinforced, impact modified nylon 6 that offers good rigidity and toughness over a wide temperature range.

Availability: Europe

Fillers/Reinforcement: Glass Fiber, 15% Filler by Weight

Additive: Impact Modifier

Features: Good Toughness; Impact Modified; Medium Rigidity

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption at Equilibrium 2.2 %50% RH; ISO 62
Linear Mold Shrinkage 0.0080 - 0.016 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13100 psiISO 527-2
Elongation at Break 9.0 %ISO 527-2
Tensile Modulus 638000 psiISO 527-2
Flexural Strength 16000 psiISO 178
Flexural Modulus 522000 psiISO 178
Izod Impact, Notched (ISO) 5.70 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) >= 21.0 ft-lb/in²ISO 180/A
Charpy Impact, Notched 7.10 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 392 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 374 °FUnannealed; ISO 72-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 482 - 536 °F
Middle Barrel Temperature 482 - 536 °F
Front Barrel Temperature 482 - 536 °F
Melt Temperature 482 - 554 °F
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F
Dry Time 20.0 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0596 / 237087

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.