MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products BC 8675E Polyurethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds for casting of concrete and plaster, does not contain MOCA, MDA, TDI or MDI. Product uses include: mold fabrication, shock absorbent pads and liners, excellent as an adhesive for high strength and resilient bonds, electrical potting and cable sealing applications, various types of urethane rubber parts.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Water Absorption 2.8 %2 weeks; ASTM D570
Brookfield Viscosity 3000 cP
Linear Mold Shrinkage 0.0015 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73 - 77ASTM D2240
Tensile Strength, Ultimate 2300 psiASTM D412
Elongation at Break 650 %ASTM D412
Tear Strength 190 pliASTM 4-624-54 D Die C
 
Processing PropertiesOriginal ValueComments
Cure Time 480 - 840 min
@Temperature 24.0 °C
demold time
 4320 - 7200 min
@Temperature 24.0 °C
full cure
Working Life 25 min
@Temperature 25.0 °C
Gel Time 40 min
@Temperature 24.0 °C
gel time (180g)
 
Descriptive Properties
Mix Ratio100:45 by weight (resin/hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products BC 8860 Polyurethane Elastomer
BCC Products BC 8690E Polyurethane Elastomer
BCC Products BC 8870 Polyurethane Elastomer
BCC Products BC 8990 Polyurethane Elastomer
Mearthane Durethane™ C 10-30A Polyurethane

PBCC066 / 107293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.