MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Texglass MV
Categories: Fluid; Lubricant

Material Notes: Texaco Texglass MV delivers value through:
  • Ability to maintain film thickness — High viscosity index indicates an oil that maintains film thickness at high temperatures.
  • Sludge protection — Detergents and dispersants minimize deposits on metal surfaces.
  • Rust protection — Contains a rust inhibitor to protect metal surfaces.
  • Long lubricant life — Resists thermal oxidation and viscosity increase, providing long lubricant life.
  • Foam inhibition

Texaco Texglass MV is a machine oil designed for use in the glass manufacturing process.

It is manufactured from highly refined mineral base oils and contains an additive package with antiwear, dispersant and detergent properties.

It has a high viscosity index to assure good film strength between metal surfaces under moderate loads and temperatures. This film strength is further enhanced by the antiwear additive protection.

The foam and aeration suppressant allows the quick release of entrained air, also improving film strength.

Texaco Texglass MV is recommended as a machine oil and constant cushion oil for I.S. glass machines. It is also designed for use in linkage and gearboxes, central lubrication systems, mechanical gob distributors, blowhead and funnel cams.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222628; MSDS Number: 8911

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 29.8 °29.8 °
Viscosity Measurement 134134Viscosity Index
Saybolt Viscosity at 100°F 572 SUS572 SUS
Saybolt Viscosity at 210°F 77.5 SUS77.5 SUS
Kinematic Viscosity at 40°C (104°F) 111 cSt111 cSt
Kinematic Viscosity at 100°C (212°F) 14.5 cSt14.5 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -38.0 °C-36.4 °F
Flash Point 234 °C453 °F
 
Descriptive Properties
Foaming Tendency, mL15Sequence II, 0 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA201 / 77080

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.