MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Total Corbion Puralact L Puralact L is a dimer of L-Lactic acid. Puralact L is a white, crystalline solid that is commonly used to prepare L-Lactide containing homopolymers or copolymers.
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Key Words: CAS L-lactide: 4511-42-6; CAS general lactide: 95-96-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 144.13 g/mol144.13 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 - 100 °C194 - 212 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.030 %<= 0.030 %
 
Component Elements PropertiesMetricEnglishComments
Tin, Sn <= 0.00020 %<= 0.00020 %
 
Descriptive Properties
AppearanceWhite Crystalline solid
Assay>99% (w/w)
Chemical Name(3S-cis)-3,6-dimethyl-1,4-dioxane-2,5-dione
Free Acid<7meq/kg
Heavy Metals<10 ppm
Meso lactide content<0.5%
Molecular FormulaC6H8O4
Stereochemical Purity>99.5% (% L-isomer)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Corbion Luminy L175 PLA, Biobased Polymer
Total Corbion Luminy LX175 PLA, Biobased Polymer
Total Corbion Luminy D070 PLA, Biobased Polymer
Total Corbion Luminy LX175U PLA, Biobased Polymer
Total Corbion Luminy D120 PLA, Biobased Polymer

PTOTAC010 / 209628

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.