System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System
Categories:
Polymer
;
Adhesive
Material Notes:
A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.
Information provided by Reltek LLC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.955
g/cc
Moisture Absorption at Equilibrium
0.040 %
@Temperature 40.0 °C
100% RH
Water Vapor Transmission
<=
2.30
g/100 in²/day
@Temperature 38.0 °C
ASTM E-96
Oxygen Transmission
350
cc-mil/100 in²-24hr-atm
@Temperature 23.0 °C
ASTM D1434
Viscosity
850
cP
Environmental Stress Crack Resistance
>=
200
hour
Mechanical Properties
Original Value
Comments
Hardness, Shore D
42
ASTM D2240
Tensile Strength at Break
900
psi
ASTM D638
Elongation at Break
350 %
ASTM D638
2% Secant Modulus
3200
psi
ASTM D790
Thermal Properties
Original Value
Comments
Crystallization Temperature
75.0
°C
Brittleness Temperature
-23.0
°C
ASTM D746
Descriptive Properties
Approximate reverse impact
24
Color
Clear
Fungi Resistance
No Growth
Insulation Resistance (V/mil)
500
Thermal Shock
No effect
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Elantas EN-8 (Conap) Casting, Potting, and Molding Compound
Valley Adhesives EM-500 High Temperature Application Glue Stick
Sika SikaTack® UltraFast Fast Cure One Part Polyurethane Adhesive
Reltek BONDiT™ B-4682 Adhesive, Sealant & Coating System
Overview of materials for Thermoset Polyurethane, Adhesive
PAQREL35 / 79999
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.