MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gold-Platinum Alloy (70Au-30Pt), Annealed at 1095°C (2000°F) then Air-Cooled
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 19.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 130
Hardness, Knoop 150Estimated from Brinell
Hardness, Rockwell A 44Estimated from Brinell
Hardness, Rockwell B 73Estimated from Brinell
Hardness, Vickers 131Estimated from Brinell
Tensile Strength, Yield 245 MPa
Modulus of Elasticity 113.8 GPaTypical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000340 ohm-cmTemperature Coefficient = 0.0059 nanoOhm-m/K between 0-1200 K
 
Thermal PropertiesOriginal ValueComments
Melting Point 1228 - 1450 °C
Solidus 1228 °C
Liquidus 1450 °C
 
Component Elements PropertiesOriginal ValueComments
Gold, Au 70 %
Platinum, Pt 30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
HGC-4 Precious dental alloy
Gold-Platinum Alloy (70Au-30Pt), Hard (66% Reduction)
Commercial Fine Gold, 60% Reduction
HGC-3-C Precious dental alloy
Wieland BioPorta G PFM Alloy

MPAuP0 / 12542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.