System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Eneos N232S Nitrile Rubber
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
Characteristics: Water resistance, Low metal corrosion
Application: O-ring, oil seal, rubber rolls, etc
ENEOS has acquired the elastomer product lines from JSR Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
0.980
g/cc
Mooney Viscosity
56
@Temperature 100 °C
ML1+4
66
@Temperature 100 °C
ML1+4, Compound (non-vulcanized)
41
@Temperature 125 °C,
Time 64800 sec
Scorch Test, ML1, Compound (non-vulcanized)
Mechanical Properties
Original Value
Comments
Hardness, Shore A
70
70
Compound (vulcanized)
58
@Temperature 40.0 °C,
Time 173000 sec
Fuel Oil B, Compound (non-vulcanized)
60
@Temperature 120 °C,
Time 252000 sec
IRM903, Compound (vulcanized)
68
@Temperature 120 °C,
Time 252000 sec
IRM901, Compound (vulcanized)
76
@Temperature 120 °C,
Time 252000 sec
Air heat Aging, Compound (non-vulcanized)
Tensile Strength
22.5
MPa
22.5
MPa
Compound (vulcanized)
10.125
MPa
@Temperature 40.0 °C,
Time 173000 sec
Fuel Oil B, Compound (non-vulcanized)
17.55
MPa
@Temperature 120 °C,
Time 252000 sec
IRM903, Compound (vulcanized)
20.925
MPa
@Temperature 120 °C,
Time 252000 sec
IRM901, Compound (vulcanized)
23.85
MPa
@Temperature 120 °C,
Time 252000 sec
Air heat Aging, Compound (non-vulcanized)
Elongation at Break
390 %
390 %
Compound (vulcanized)
214.5 %
@Temperature 40.0 °C,
Time 173000 sec
Fuel Oil B, Compound (non-vulcanized)
273 %
@Temperature 120 °C,
Time 252000 sec
IRM901, Compound (vulcanized)
284.7 %
@Temperature 120 °C,
Time 252000 sec
IRM903, Compound (vulcanized)
284.7 %
@Temperature 120 °C,
Time 252000 sec
Air heat Aging, Compound (non-vulcanized)
100% Modulus
3.60
MPa
Compound (vulcanized)
300% Modulus
18.4
MPa
18.4
MPa
Compound (vulcanized)
Resilience
34
[%], Rebound, Compound (vulcanized)
Tear Strength
51.0
kN/m
Compound (vulcanized)
Compression Set
12 %
@Temperature 100 °C,
Time 252000 sec
Compound (vulcanized)
19 %
@Temperature 120 °C,
Time 252000 sec
Compound (vulcanized)
Thermal Properties
Original Value
Comments
Brittleness Temperature
-27.0
°C
Descriptive Properties
Acrylonitrile Content (%)
35
Delta;V
100
(%)
1
IRM901 70 hrs at 120°C, Compound (vulcanized)
1
Distilled Water 70 hr at 40°C, Compound (non-vulcanized)
16
IRM903 70 hrs at 120°C, Compound (vulcanized)
28
Fuel Oil B 48 hrs at 40°C, Compound (non-vulcanized)
50
Fuel Oil C 48 hrs at 40°C, Compound (non-vulcanized)
88
Fuel Oil C/Ethanol 48 hrs at 40°C, Compound (non-vulcanized)
Extrusion Test
118
80°C, 25 rpm, Die Swell %
322 cm/min
80°C, 25 rpm, Extrusion Length
352 cc/min
80°C, 25 rpm, Extrusion Volume
Flex Test
10
Occurrence(Thousand Times)
3
Growth 2 to 15 mm (Thousand Times)
Flow Rate
39
Q×10
4
, 80°C, 100 kg, Kokahiki Flow tester
JSR Mold Curast Test 160°C, Minutes
2
t
c(10)
5
t
c(90)
Low-Temperature Torsion Test
-23°C
t10
-27°C
t100
Mill Contraction 50°C (%)
46
Ozone Degradability Test
C-3
Static 20% Elongation, 50 ppm 5 Hours at 40°C
C-3
Dynamic 0 to 20% Elongation, 50 ppm 5 Hours at 40°C
Product form
Bale
Product Stain
NS
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PJSRC8058 / 295374
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.