Product Description: LLB100-B is a general-purpose film grade linear low density polyethylene. This resin exhibits excellent toughness and strength when drawn down to gauges. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America Additive: Antiblock: No; Slip: No Features: Butene Comonomer; General Purpose; High Strength; High Toughness Uses: Bags; Blending; Loners; Packaging Processing Method: Extrusion Information provided by Osterman & Company |