MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Pearlbond™ 5713 F1 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlbond™ 5713 F1 TPU is a Polyester-Type Thermoplastic Polyurethane (TPU).

Description: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and bond strengths can be achieved with the addition of diisocyanates, peroxides, epoxies and polyfunctional amides.

Uses: Hot melt adhesive, solution cast films for lamination on fabrics.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D-792
Viscosity 130000 cP
@Temperature 204 °C
130000 cP
@Temperature 399 °F
ASTM D-1084-88
Brookfield Viscosity 800 - 1300 cP800 - 1300 cP15% T.S. in THF
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D-2240
Hardness, Shore D 4545ASTM D-2240
Tensile Strength 37.9 MPa5500 psiASTM D-412/D-638
Elongation at Break 600 %600 %ASTM D-412/D-638
100% Modulus 4.70 MPa
@Strain 100 %
682 psi
@Strain 100 %
ASTM D-412/D-638
300% Modulus 9.00 MPa
@Strain 300 %
1310 psi
@Strain 300 %
ASTM D-412/D-638
Peel Strength 0.400 kN/m2.28 pliT-peel, Aluminum Foil; ASTM D-1876-72
 5.30 kN/m30.2 pliT-peel, Mylar Film; ASTM D-1876-72
 7.20 kN/m41.1 pliAdhesion to Peel; TP-141
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 95.0 °C203 °FASTM D-1525
Glass Transition Temp, Tg -43.0 °C-45.4 °F
Ring & Ball Softening Point 170 °C338 °FASTM E-28-92
 
Descriptive Properties
Gradient Bar Tack Temperature84°C
Open Time>315 secASTM D-4497-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5040 / 238910

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.