Lower cost paper phenolic NEMA Grade XP. NP660 uses natural kraft paper without pigmented cover sheet. It is a warm to hot punching material. It is available in natural and black only, without a pigmented cover, only.Information provided by Norplex-Micarta |
Paper, Phenolic, Micarta, NEMA XP, MIL-I-24768/19 - PBM-P, ASTM D709 Type I Grade XP |