MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker EL R 1188 GRY TS Silicone Rubber Compound
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: EL R 1188 GRY TS *BULK, INT is a silicone rubber compound designed specifically or use in high voltage applications. It cures to an elastomer of high hardness with very good electrical properties. It is an excellent material for insulators and cable accessories.

Special features:

  • Good physical profile
  • Excellent arc resistance
  • Good extrusion qualities
Application: EL R 1188 GRY TS *BULK, INT Silicone Rubber Compound is designed specifically for use in high voltage applications. Suspension and line post insulators and surge arrestors molded from EL R 1188 GRY TS *BULK, INT possess excellent resistance to arcing and tracking, increasing the reliability and reducing power interruptions.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ISO 868
Tensile Strength at Break 0.650 MPaISO 37
Elongation at Break 225 %ISO 37
Tear Strength 75.0 pliASTM 624 B
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9077 / 204606

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.