MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Fainplast Compounds HAX HF 018/25 Halogen Free PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Insulation; very low thickness

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 - 1.53 g/cc0.0538 - 0.0553 lb/in³IEC 60811
Melt Index of Compound 10 g/10 min
@Load 21.6 kg,
Temperature 150 °C
10 g/10 min
@Load 47.6 lb,
Temperature 302 °F
Fainplast
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 5650 - 56IEC 60811
Tensile Strength at Break 11.0 MPa1600 psiIEC 60811
Elongation at Break 140 %140 %IEC 60811
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm
@Temperature 20.0 °C
1.00e+15 ohm-cm
@Temperature 68.0 °F
ASTM D257
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 35 %35 %ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fainplast Compounds FK 86 Flexible PVC, Insulation Lead Free
Fainplast Compounds FK 90 Flexible PVC, Insulation Lead Free
Geon® Performance Solutions Vinyl Wire & Cable JJC32A Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJJC310L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJJC32L Polyvinyl Chloride, Flexible

PFAIN693 / 80895

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.