MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 9737 Double Coated Splicing Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrier

Features:

  • High tack, acrylic adhesive offers good low and elevated temperature resistance.
  • Adheres well to both kraft and coated papers
  • High performance splicing tape for use on paper, plastics and other continuous web processes.
  • Electronics, General Industrial, Appliances, Medical Devices, Power Tools, Automotive, Transportation, Aircraft, Airplane
  • Adhering, joining, affixing, bonding, mounting, holding, laminating, and attaching

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.7 microns0.500 milCarrier
 81.3 microns3.20 milLiner
 88.9 microns3.50 milTape
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.657 kN/m3.75 plito Steel, Initial at RT
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 127 °C261 °FLong term
 149 °C300 °FShort term
Minimum Service Temperature, Air -23.0 °C-9.40 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear
Liner55# Densified Kraft Paper, White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33290 / 168037

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.